Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEX NORYL™ Resin WCD883CU - Asia - (PPE+TPE) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for FLEX NORYL™ Resin WCD883CU - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flex Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
FLEX NORYL™ WCD883CU resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This UV stabilized material contains non-halogenated flame retardant and performance capable of meeting EN 50265-2-1 requirements. FLEX NORYL WCD883CU resin was developed for evaluation in AC cable jacket applications such as HD 21.14 flexible cables that require EU VDE and light color. It has a Shore A Hardness reading of 88 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 10 g/10min ASTM D 1238
온도 250 °C -
하중 10 kg -
기계적 특성단위시험규격
ISO 데이터
파단시 강도 12.5 MPa ISO 527
파단시 신율 50 % ISO 527
ASTM 데이터
파단시 강도 14 MPa ASTM D 638
파단시 신율 160 % ASTM D 638
쇼어 A 경도 88 - ASTM D 2240
열적 특성단위시험규격
ISO 데이터
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
전기적 특성단위시험규격
ISO 데이터
CTI 600 - IEC 60112
ASTM 데이터
표면 저항 >1E15 Ohm ASTM D 257
부피 저항 >1E15 Ohm*cm ASTM D 257
기타 특성단위시험규격
밀도 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Screw speed 15 - 85 rpm -
특징
부가물
난연제
특별 특성
난연성
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com